Product description
1) Please spray some water on dried cement's surface after completed the work to avoid the cement's surface too dry that can cause powder produced on surface.
2) Please do not add water when the mixed cement starts to dry, because it may reduce the strength/ performance of cement.
3) The cement can mix with sand or normal cement, but the drying time will take longer time instead of few minutes. Therefore, we are suggested to add normal cement to increase the drying time, if cannot handle quick drying speed of Quick Dry Cement.
4) Please mix the 3 minutes Quick Dry Cement and water based on ratio (Cement: Water= 1: 0.3) within 1 minute to avoid the cement dried before applying.
5) Please follow the cement-water ratio and do not add too more water, as more water will reduce hardness and increase the
drying time/speed of cement.
6) Due to cement is powder and will release heat in drying process, please be careful during the work (wear mask and gloves)
1. Kalis air n kalis kebocoran utk tandas, dapur, ruang bawah tanah, dinding, kolam, paip, terowong, dil.
2. Bersihkan permukaan supaya bebas dri benda longgar n kesan minyak. Lembapkn permukaan selepas simen
3. Pahat tempat kebocoran ke port berbentuk "V" atau "U".
4. Gaulkan ke dlm bentuk, selepas mula mengeras, tampal simen ke dlm tempat yng bocor n peras dgn kayu
utk menekannya ke dlm n sekelilingnya, dan ia akn menghentikn kebocoran serta-merta.
1. Setelah simen telah keras, lembabkannya dgn segera utk mengelakkan menjadi kapur atau mula jatuh dari
2. Kaedah melembabkan permukaan dapat dibahagikan kepada: menyemburkn air, menutup benda basah, menutup
kain plastik n lain2. Simen menyembuhan keseluruhannya dlm 2-3 ari